Trademark | Code | Applications |
HT200 | C.I. | Water below 80 ℃ |
GCr15 | GCr15 | Bearing steel |
QT500 | QT | Water pump housing |
ZG230-450 | ZG25 | Water, oil |
42CrMo | 4140 | Shaft |
1Cr13 | 410 | Food, oil |
2Cr13 | 420 | Shaft |
1Cr13Ni | 410S | High-pressure water pump housing, balance disc, etc. |
1Cr18Ni9 | 302 | Alkaline, acidic water |
0Cr18Ni9 | 304 | Alkaline, acidic water |
1Cr18Ni12 | 305 | Acidic water |
0Cr25Ni20 | 310S | Caustic soda |
1Cr18Ni12Mo2Ti | M | Dilute sulfuric acid, phosphoric acid, organic acids |
00Cr17Ni14Mo2 | 316L | Dilute nitric acid, phosphoric acid, organic acid |
00Cr19Ni13Mo3 | 317L | Ibid, resistance to intergranular corrosion |
1Cr18Ni9Ti | 321 | Alkaline, acidic water, organic acids |
00Cr20Ni25Mo4.5Cu | 904L | Various concentrations of sulfuricacid below 70 ℃ |
0Cr30Ni42Mo3Cu2 | 804 | Caustic soda 150 ℃ |
0Cr20Ni42Mo3Cu2 | 824 | 904 is still impatient corrosion |
0Cr21Ni32Mo2Cu3 | 20 # alloy | Hot concentrated sulfuric acid, T ≤ 130 ℃, 40% concentration |
0Cu24Ni20Mo2Cu3 | K alloy | ≤ 60% of various concentrations of sulfuric acid |
00Cr10Ni20Si6Mo | 920 | Hot concentrated sulfuric acid, T ≤ 130 ℃, the concentration of 93-98% |
00Cr25Ni6Mo2 | MM-4 | Special steel nitrophosphate |
0Cr17Ni7Al | 631 | The long axis of liquid pumps |
N6 | Pure Nickel | High temperature caustic soda, alkali evaporator |
0Ni60Mo22Fe20 | Hastelloy A | Various concentrations of hydrochloric acid below 70 ℃ |
00Ni65Mo28 | Hastelloy B | All concentrations of hydrochloric acid |
0Ni60Mo18Fe8Cr17Cu3Mn | Hastelloy C | Cold nitric acid, hypochlorous acid,hydrofluoric acid, etc. |
00Cr30Ni40Mo4Cu3 | Lewmet55 | All full-temperature sulfuric acid concentration |
00Ni65Cu28 | Monel | Hydrofluoric acid, silicon fluoride acid, high temperature caustic soda |
00Cr14Ni14Si4 | C4 | Full concentration of nitrate |
TiAl6V4 | TC4 | Oxidizing corrosive media |
TA2 | Ti | Mother liquor of soda ash, sea water |
0Cr26Ni5Mo2Cu3 | CD4MCu | Solid containing dilute sulfuric acid, phosphoric acid, wear and corrosion |
F30%CrMo | Cr30 | Phosphoric acid slurry, more wear and corrosion |
00Cr25Ni6Mo2 | MM-4 | Nitrate, phosphate-specific |
0Cr27Ni31Mo4.5Cu2 | ZS28 | Hydrochloric acid slurry |
STSi15 | G | Nitric acid, chromic acid, sulfuric acid, etc. (excluding HCl) |
Cr28 | E | Concentrated nitric acid |
Cr30 | F30%CrMo | For corrosive and abrasive media |
0Cr18Ni5Mo5 | NH55 | Seawater |
00Cr22Ni5Mo3N | SAF2205 | Seawater |
00Cr25Ni7Mo4N | SAF2507 | Water, better than SAF2205 |
0Cr17Ni17Si5 | 05 | High concentration, high temperature sulfuric acid |
1Cr26Ni6 | PH50 | Casing wear ring |
STNiCr202 | Nickel-iron | High temperature and high concentration of caustic soda |
TiMo32 | 32 Mo Titanium Alloy | Oxidation and reduction of corrosive media |
TiMo0.3Ni0.8 | Ti, Mo, Ni alloys | Oxidative corrosion medium, crevice corrosion resistance |
TiTa5 | Titanium tantalum alloys | Hot concentrated nitric acid and synthetic resins and other strong corrosive media |